Veronika
desde
United Kingdom
asks
Hello! Is this clay ready to throw straight from the bag or does it need wedging? The same question applies to several other Scarva clays. Many thanks :)
Respuestas de Scarva:
|
Yes it should be fine, some people like to wedge the clay to bring it to their desired consistency but in most cases this is not necessary, hope this helps.
|
James
desde
United Kingdom
asks
Would this be the clay to puddle with sand if I were to build a pizza oven?
Respuestas de Scarva:
|
We have made a clay especially for creating a pizza oven. Here is the link:
https://www.scarva.com/en/Scarva-Earthstone-ES180-Sculpting--Pizza-Body-Clay/m-20.aspx
|
Senay
desde
United Kingdom
asks
Hi,
How much shrinks after firing? Thank you.
Respuestas de Scarva:
|
Hi,
Approx 14% at 1100°C
Hope this helps!
|
calista
desde
United Kingdom
asks
what's an ideal bisque firing temp range for this clay? 1050 seems high?
Respuestas de Scarva:
|
Hi, we recommend all bisque firings to 1000°C
Hope this helps!
|